The concentrate produced from the scavenger cleaner circuit, representing roughly 12% of the mill feed, will be reground to a P80 of 10 µm prior to final cleaning in the low entrainment scavenger recleaner stage. The scavenger recleaner concentrate then will be combined with the highgrade cleaner concentrate to form the final concentrate.